Skip to main content
. 2012 Dec 6;2(4):841–854. doi: 10.3390/membranes2040841

Figure 2.

Figure 2

Particle size distributions of catalyst inks pre-heated at (a) 25 °C; (b) 50 °C and (c) 80 °C.