1H NMR T1, and ionic conductivity values for Nafion 117 membrane heat-treated at 25, 50, and 80 °C.

Sample Name Heat-Treatment Temperature (°C) Nucleus (1H)
T1 (s) Ionic Conductivity (S/cm)
Nafion 117 membrane (ref.) 0.22 0.062
A 25 0.25 0.079
B 50 0.20 0.079