Table 1. Comparison of our YSCs with the reported YSCs in terms of C and E.
Ref. | Electrode materials |
C |
E |
|||
---|---|---|---|---|---|---|
CA (mF cm−2) | CV (F cm−3) | CL (mF cm−1) | EA (μWh cm−2) | EV (mWh cm−3) | ||
This study | RGO+CNT | 177 | 158 | 5.3 | 3.84 | 3.5 |
1 | Pen ink | 26.4 | 1.008 | 2.7 | ||
3 | Graphene | 1.7 | 0.17 | |||
5 | PANI/CNT | 38 | ||||
7 | CNT/OMC | 39.7 | 1.91 | 1.77 | ||
8 | CNT/MnO2 | 3.01 | 0.015 | 1.73 | ||
10 | PEDOT/CNT | 73 | 179 | 0.47 | 1.4 | |
11 | ZnO nanowires/MnO2 | 2.4 | 0.04 | 0.027 | ||
31 | CNT and Ti fibres | 0.6 | 0.024 | 0.15 | ||
32 | Graphene | 0.726 | 0.01 | |||
33 | ZnO nanowires/graphene | 2 | 0.025 | |||
38 | PANI/stainless steel | 41 | 0.95 | |||
39 | Carbon/MnO2 | 2.5 | 0.22 |
CNT, carbon nanotube; OMC, ordered mesoporous carbon; PANI, polyaniline; PEDOT, poly(3,4-ethylenedioxythiophene); YSC, Yarn supercapacitor.