. 2013 Aug 28;4(3):162–177. doi: 10.3390/jfb4030162

Figure 1.

Figure 1

Degradation profile of 10% w/w BDDGE cross-linked hydrogels after exposure to collagenase and compared to EDC/NHS cross-linked hydrogels.