Figure 2.

(a), (b), and (c) show higher magnification SEM micrographs of the S3 surface, respectively, after soaking in SBF solution for 7 days showing the apatite forming ability of the scaffolds.

(a), (b), and (c) show higher magnification SEM micrographs of the S3 surface, respectively, after soaking in SBF solution for 7 days showing the apatite forming ability of the scaffolds.