. 2014 May 23;9:2439–2458. doi: 10.2147/IJN.S58487

Figure 11.

Figure 11

Mechanical properties of glutaraldehyde vapor crosslinked gelatin nanofibers with and without drug loading. The gelatin fiber mat was crosslinked with glutaraldehyde for 48 hours. For amphotericin B- and natamycin-loaded gelatin fiber mats 3-hour glutaraldehyde crosslinking was used.

Abbreviation: AmpB, amphotericin B.