Skip to main content
. 2014 May 29;9(1):266. doi: 10.1186/1556-276X-9-266

Figure 6.

Figure 6

Hysteresis loops and temperature dependence of magnetization. (a) Hysteresis loops obtained at 300 and 2 K for the as-grown and annealed films with external field applied parallel to EuTiO3[100] direction. The inset magnifies the low magnetic field range. (b) Temperature dependence of the magnetization curves of the as-grown and annealed films at 1,000 Oe and 20 kOe external fields applied parallel to EuTiO3[100] direction.