. 2014 Jun 1;3(3):117–126. doi: 10.1089/biores.2014.0015

Table 2.

Shrinkage, Initial Mass, Mass After Treatment, and Water Absorption of Electrospun PLGA Scaffolds

Sample groups Shrinkage (%) Initial mass (mg) Mass after treatment (mg) Water absorption (%)
PLGA 0 4.11±0.77 0 0
PLGAH01 14 4.52±0.65 21.24±2.5 373.7±55.5
PLGAH001 19 4.34±0.54 5.4±0.86 24.3±11.6
PLGAH01FN 27 4.3±0.71 21.28±4.6 402.8±108.5
PLGAH001FN 36 4.2±0.55 6.7±1.3 61.1±32.9

Data are expressed as mean±SD.