Figure 1. XRD pattern of five adsorbent composites: (a) uncalcined Fe3O4-HBC composite, (b) 400°C under air, (c) 400°C under nitrogen, (d) 1000°C under air, and (e) 1000°C under nitrogen. Different XRD peaks are also marked.