Skip to main content
. 2014 May 28;5:726–734. doi: 10.3762/bjnano.5.85

Figure 4.

Figure 4

IV characteristics of graphene and CNT after exposure to NH3 under F = 500 ppm at (a) T = 25 °C, (b) T = 50 °C, (c) T = 100 °C, (d) T = 150 °C.