Figure 5. The etched surfaces of the scaffolds without the second sintering step (a); sintered at T2 of 1100 (b) °C, 1150°C (c), 1200°C (d), and 1250°C (e); and the average grain sizes of the scaffolds prepared using SLS without the second sintering step and of those using NTSS at different T2 (f).