Skip to main content
. 2014 Jun 6;6(13):10238–10247. doi: 10.1021/am501568j

Figure 5.

Figure 5

(a) Scheme of intercalation into PbI2 film coated with Al metal strips. (b) PL line mapping performed from the backside of the glass substrate and the corresponding confocal PL images obtained using a 410 nm diode laser. (c, d) Corresponding PL image plot and PL peak intensity across the structures.