Skip to main content
. Author manuscript; available in PMC: 2015 Aug 1.
Published in final edited form as: Biomaterials. 2014 May 16;35(25):6787–6796. doi: 10.1016/j.biomaterials.2014.04.083

Fig. 2. Phase 1 Neotissue Functional Properties at t = 6 and 12 wk.

Fig. 2

Collagen content per construct wet weight (A), pyridinoline content per construct wet weight (B), Young’s modulus (C), and ultimate tensile strength (D) of untreated, LOX, C-ABC+TGF-β1, and LOX+C-ABC+TGF-β1 neofibrocartilage at t = 6 and 12 wk. Bars not connected by the same letter are significantly different (p < 0.05), lower case letters denote significant differences for 6 wk constructs, upper case letters denote significant differences for 12 wk constructs, n = 6 per group, mean ± SD.