Skip to main content
. 2014 Jul 14;9(1):350. doi: 10.1186/1556-276X-9-350

Figure 5.

Figure 5

SEM pictures of grooved nanofibers electrospun from 10% PS solution. (A, B) Grooved nanofibers and (C) cross section. THF/DMF ratio 1:1 v/v, RH 40%, collecting distance 15 cm, feeding rate 1.5 ml/h, and applied voltage 12 kV.