SEM pictures of the surface of the FTO glass substrates after electrolysis for 20 s (a) and 30 s (b) in an ethanol/water (75/25, v/v) mixed solution containing 3 mM Cu(ClO4)2, 9 mM LiSCN, 0.1 M LiClO4, and 1.0 mM RB.