Skip to main content
. 2014 Jul 17;2014:542678. doi: 10.1155/2014/542678

Table 3.

Flexural modulus mean and standard deviation (GPa) for the interaction between %wt of glass fibers and type of resinous material. Statistical comparisons by ANOVA following Tukey HSD test and paired comparisons by Student t-test (α = 0.05).

Quantity of glass fibers (%wt) Type of resinous materials
Filled resin Unfilled resin
0 2.06 ± 0.88Ba 1.01 ± 0.71Cb
10 4.48 ± 3.02ABa 7.03 ± 7.86BCa
15 5.69 ± 2.79Ab 19.33 ± 16.75ABa
20 6.04 ± 3.39Ab 15.72 ± 8.03ABa
30 2.49 ± 1.34Bb 29.36 ± 13.92Aa

Different capital letters (vertical analysis) and lower case letters (horizontal analysis) mean statistical significant differences with P < 0.05.