Table 2.
Percentage crystallinity (%Cr) and crystalline index (C.I.) of raw, delignified and graft copolymers prepared under the influence of MWR.
Sample name | Pg | At 2θ scale | % Cr | C.I. | |
---|---|---|---|---|---|
I22 | I15 | ||||
Raw Grewia optiva fiber | – | 903 | 432 | 67.64 | 0.52 |
Delignified Grewia optiva fiber | – | 396 | 158 | 71.48 | 0.60 |
dGo-g-poly(MMA) | 26.54 | 467 | 216 | 68.37 | 0.53 |
dGo-g-poly(MMA-co-EMA) | 51.56 | 511 | 428 | 54.41 | 0.48 |
dGo-g-poly(MMA-co-EA) | 86.32 | 508 | 472 | 51.31 | 0.43 |