. 2013 Dec 18;20(15-16):2077–2087. doi: 10.1089/ten.tea.2013.0358

FIG. 2.

FIG. 2.

(a) β-TCP scaffold fabricated via SFF. (b–c) Incubation of β-TCP scaffolds in mSBF for 7 days resulted in the formation of a continuous coating. (d) The morphology of the mineral displayed a plate-like nanostructure characteristic of hydroxyapatite. β-TCP, beta tricalcium phosphate; mSBF, modified simulated body fluids; SFF, solid-free form fabrication.