Table 2.

Water swelling capacity and relative enzyme adsorption of the NMMO pretreated and untreated pinewood.

Pretreatment Wood size Water swelling capacity
(g water/g wood)1
Relative enzyme adsorption2
Untreated Powder 7.2 4.0
Pretreated for 1 h Powder 10.0 4.9
Pretreated for 3 h Powder 10.7 5.2
Pretreated for 15 h Powder 11.0 6.7

Untreated chips 1.0 1.0
Pretreated for 1 h chips 2.0 1.5
Pretreated for 3 h chips 3.7 2.7
Pretreated for 15 h chips 3.8 4.3

1The standard deviation of all samples was less than 6.3%.

2The standard deviation of all samples was less than 7.2%.