Electrochemical maps and line scans of a pristine SWNT before (a) and after (b) electrochemical oxidation; start and end potential 0 V, return potential 1.30 V at a scan rate of 50 mV/s (inset of (a)). Maps obtained at −0.75 V vs Ag/AgCl QRCE.