Skip to main content
. 2014 Aug 15;9(1):398. doi: 10.1186/1556-276X-9-398

Figure 3.

Figure 3

AFM images of MIFs. The MIFs were prepared using annealing in hydrogen at 250°C and coated with 3-nm (top left), 10-nm (top right), 50-nm (bottom left), and 200-nm (bottom right) TiO2.