Table 2.

Means of microtensile bond strength values (± standard error) in MPa for adhesives All Bond 3 and Excite, considering different surface treatments and storage time. 2-Way ANOVA applied separately for each adhesive.

SURFACE TREATMENT ALL BOND 3 EXCITE
24 hours 6 months 15 months 24 hours 6 months 15 months
WATER 51.07 (3.6)A,a 57.13 (3.6)A,a 47.29 (4.4)A,a 49.51 (5.4)AB,a 42.10 (5.4)AB,a 45.51 (6.6)A,a
CHD/WATER 46.96 (3.6)A,a 50.69 (3.6)A,a 46.07 (4.4)A,a 40.05 (5.4)B,a 36.78 (5.4)B,a 40.87 (6.6)A,a
ETHANOL 59.41 (3.6)A,a 56.41 (3.6)A,a,b 44.41 (4.4)A,b 49.67 (5.4)AB,a 44.56 (5.4)AB,a 42.48 (5.4)A,a
CHD/ETHANOL 54.67 (3.6)A,a 52.17 (3.6)A,a,b 39.58 (4.4)A,b 53.37 (5.4)A,a 57.47 (5.4)A,a 49.55 (6.6)A,a

Different superscript letters represent values significantly diferentes (p<0,05) for All Bond 3. Capitalized letters compare treatments and lower cases compare storage periods.

Different superscript letters represent values significantly diferentes (p<0,05) for Excite. Capitalized letters compare treatments and lower cases compare storage periods.