Skip to main content
. Author manuscript; available in PMC: 2015 Oct 1.
Published in final edited form as: Acta Biomater. 2014 Jun 28;10(10):4136–4142. doi: 10.1016/j.actbio.2014.06.032

Fig. 2.

Fig. 2

NO surface flux from SG-80A and SP-60D-20 films doped with 25 wt% DBHD/N2O2 and 10 wt% 5050DLG1A (1-2 week hydrolysis rate) PLGA additives. Films were incubated in PBS buffer at 37°C during the testing period. The data are means ± SEM (n=3).