Skip to main content
. 2014 Sep 23;9(9):e106754. doi: 10.1371/journal.pone.0106754

Figure 2. XRD powder patterns of unhydrated cements and hydrated PSCs stored in D.I. water for 1, 3 and 7 day.

Figure 2