Figure 4.
Compressive strength comparison of the scaffolds sintered at 1150 °C (a), and 1250 °C (b) in conventional and microwave furnace (**p < 0.05, *p > 0.05, n = 10).
Compressive strength comparison of the scaffolds sintered at 1150 °C (a), and 1250 °C (b) in conventional and microwave furnace (**p < 0.05, *p > 0.05, n = 10).