Published in final edited form as: J Tissue Eng Regen Med. 2012 Mar 7;7(8):631–641. doi: 10.1002/term.555

Table 3.

Designed porosity (%) and calculated total sintered open porosity (%).

Designed Pore Size Sintering Temperature Sintering Method Bulk Density (%) Total Open Porosity (%) Designed Porosity
500 μm 1150 °C CS 32.02 ± 2.28 57.87 ± 2.63 27%
MW 38.67 ± 1.35 51.4 ± 3.1
1250 °C CS 37.69 ± 0.63 54.11 ± 3.97
MW 42.95 ± 1.60 42.75 ± 0.99
750 μm 1150 °C CS 28.22 ± 1.19 63.1 ± 0.26 35%
MW 33.95 ± 1.26 59.76 ± 1.42
1250 °C CS 30.80 ± 0.29 58.61 ± 5.35
MW 39.97 ± 3.83 46.98 ± 5.24
1000 μm 1150 °C CS 32.91 ±0.16 63.83 ± 5.17 41%
MW 35.16 ± 0.86 57.74 ± 4.64
1250 °C CS 26.89 ± 1.42 58.22 ± 0.39
MW 24.23 ± 1.35 54.27 ± 4.05