Skip to main content
. 2014 Jan 13;30(5):1391–1400. doi: 10.1021/la403666y

Figure 8.

Figure 8

In situ tapping-mode AFM brush height determined over a relatively narrow pH window for micropatterned PTBAEMA brushes immersed in aqueous solution: (■) linear PTBAEMA brush (original dry brush thickness = 13 nm); (●) uniformly cross-linked PTBAEMA brush prepared using PPG-TDI in THF; (⧫) surface-cross-linked PTBAEMA brush prepared using PPG-TDI in n-hexane.