Table 1. Size, Polydispersity, and Surface Charge of UPE Nanoparticles Measured by DLS before and after Surface Modification.
sample | Dav [nm] | polydispersity [PD] | zeta potential [mV] |
---|---|---|---|
control NPs | 420 | 0.335 | –47.0 |
MTNs | 450 | 0.357 | –49.0 |