Figure 2.

Figure 2

Scattering spectra from tetra-functional PEG hydrogels formed with 4K, 8K, 12K, and 35K MW PEG with varying initial polymer concentrations between 0.077 g/mL and 0.50 g/mL. Spectra have been shifted for clarity.