Skip to main content
. 2014 Nov 4;10:2573–2579. doi: 10.3762/bjoc.10.269

Table 1.

Conditions and results of ring-opening polymerization from pPR.

polymerization conditions GPR
run Mn Mw Yielda

1 60 °C, 48 h 97,000 115,000 69%
2 rt, 6 h → 40 °C, 24 hb 181,000 209,000 33%
3 rt, 48 h 167,000 197,000 3%
4 130 °C, 10 h (11,000)c (15,000)c 0%
5 0 °C, 7 h (780)c (850)c 0%

aYields based on polymer backbone. bTemperature increased after 6 h. cMolecular weights of byproducts.