Table 5.
Dry reforming reactions reported in literature using metals (other than nickel) at different temperatures (T), gaz hourly space velocity (GHSV), with different pressures (P), and reported Time On Stream (TOS).
| Catalyst | Conditions | CH4/CO2 conversion H2/CO ratio TOS | References |
|---|---|---|---|
| CeO2 | T = 900°C | 32%/nd | Laosiripojana and Assabumrungrat, 2005 |
| GHSV = 4 | 0.93 | ||
| [O] = CO2 | 10 h | ||
| P = 1 atm | |||
| Mo2C | T = 947°C | 90%/93% | Brungs et al., 2000 |
| SiO2, Al2O3, TiO2, ZrO2 | GHSV = 2.6 | 0.95 | |
| [O] = CO2 | 40 h | ||
| P = 7.9 atm | |||
| Ru | T = 750°C | 57%/nd | Ferreira-Aparicio et al., 2000 |
| SiO2, Al2O3 | GHSV = 120 | nd | |
| [O] = CO2 | 10 min | ||
| P = nd | |||
| VC, NbC, TaC | T = 1050°C | 90%/90% | Brungs et al., 1999 |
| GHSV = 1.2 | 0.96 | ||
| [O] = CO2 | 25 h | ||
| P = 7.9 atm | |||
| Ru, Rh, Pt | T = 850°C | 95%/nd | Tsyganok et al., 2004 |
| Mg(Al)OX | GHSV = 227 | 1.8 | |
| [O] = CO2 and O2 | 5 h | ||
| P = 1 atm | |||
| Co | T = 800°C | 95% + /95% + | Bouarab et al., 2004 |
| MgO-SiO2 | GHSV = 13 | 1.12 | |
| [O] = CO2 | 13 h | ||
| P = 1 atm | |||
| CoNdOx | T = 850°C | 92%/92% | Choudhary et al., 2005 |
| GHSV = 20 | 0.91 | ||
| [O] = CO2 | 60 h | ||
| P = 1 atm | |||
| Ir/Ce0.9Gd0.1O2−x | T = 800°C | 65%/85% | Wisniewski et al., 2005 |
| GHSV = 30 | 0.9 | ||
| [O] = CO2 | 20 | ||
| P = 1 atm | |||
| Pt | T = 700°C | 80%/80% | Özkara-Aydınoğlu et al., 2009 |
| ZrO2 | GHSV = 15.6 | 1 | |
| Ce (promoter) | [O] = CO2 | 4 | |
| P = 1 atm |
*GHSV, Gas hourly space velocity expressed in l/gcat*h.