Properties of MPRs used in the present study

Items Matrix structure Density (g/mL) Particle size (μm) Specific surface area (m 2 /g) Porosity (%) Average pore diameter (nm)
D3520
Crosslinked Polystyrene
1.02-1.06
300-1250
480-520
65-70
8.5-9.0
D4020
Crosslinked Polystyrene
1.08-1.12
300-1250
540-580
46-50
10-10.5
NKA
Crosslinked Polystyrene
1.02-1.06
300-500
570-590
78-80
20-22.0
AB-8
Crosslinked Polystyrene
1.02-1.08
480-520
480-520
42-46
13-14.0
NKA-9 Crosslinked Polystyrene 1.02-1.04 300-700 540-580 74-78 15.5-16.5