Skip to main content
. 2014 Oct 7;15(11):4046–4053. doi: 10.1021/bm501091p

Figure 3.

Figure 3

(a) DLS profile (PDI = 0.457) of the nanogel after 48 h incubation at pH 5. (b) TEM image of the nanogel after 48 h incubation at pH 5; temperature = 25 °C.