Published in final edited form as: Adv Funct Mater. 2009 Mar 9;19(8):1276–1286. doi: 10.1002/adfm.200801561

Figure 6. Thickness increase of the two-layer hydrogels with PFM in water compared with the HEMA-co-EGDA hydrogel.

Figure 6

(A) Decrease of the swelling ability for two samples with different crosslink degrees, EGDA/HEMA = 0.01 and 0.17. (B) Thickness increase as