Skip to main content
. Author manuscript; available in PMC: 2015 Oct 5.
Published in final edited form as: J Appl Polym Sci. 2014 May 6;131(19):10.1002/app.40879. doi: 10.1002/app.40879

FIGURE 10.

FIGURE 10

Confocal microscopy images of materials, post-cure, having undergone PIPS; scale bar represents 50 µm. A) TEGDMA, DC=77 %, B) TEGDMA/1 wt% PMMA (3:1), DC=82 %, C) TEGDMA/3 wt% PMMA (3:1), DC=93 %, D) TEGDMA/5 wt% PMMA (3:1), DC=85 %, E) TEGDMA/10 wt% PMMA (3:1), DC=75 %, F) TEGDMA/20 wt% PMMA (19:1), DC=70 %.