Figure 1.

Figure 1.

Scanning electron micrographs showing the effect of sintering temperature on grain size in 3Y-TZP sintered for 2 hr. (A) 1,300°C; (B) 1,350°C; (C) 1,400°C; (D) 1,450°C; (E) 1,500°C; (F) 1,550°C; (G) 1,600°C; and (H) 1,650°C.