Table 1.
Number of specimens used for s-GAG and hydration measurements | |||
---|---|---|---|
| |||
Control | Buffer-treated | Enzyme-treated | |
s-GAG | n = 6 | n = 6 | n = 6 |
Hydration | n = 6 | n = 6 | n = 6 |
Number of specimens used for the measurement of thickness and mechanical behavior changes | |||
| |||
Control/Buffer-treated | Buffer-treated/Enzyme-treated | ||
| |||
Mechanical changes | n = 5 | n = 7 | |
Thickness change | n = 8* | n = 9# |
The * denotes that 5 of the 8 specimens used to measure the thickness change were used for mechanical testing. Similarly, the # denotes that 7 of the 9 specimens used to measure the thickness change were subjected to mechanical testing.