Table 1.
Elastic modulus (MPa) | Yield strength (MPa) | |||||
---|---|---|---|---|---|---|
| ||||||
PR model | Experiment | Voxel model | PR model | Experiment | Voxel model | |
| ||||||
PT | 757 ± 383 | 785 ± 407c | 739 ± 387c | 3.98 ± 2.11b | 4.09 ± 2.32c | 5.12 ± 2.72b,c |
FN | 3,239 ± 1,518 | 3,132 ± 1,466 | 3,155 ± 1,447 | 18.68 ± 8.83b | 18.72 ± 8.88c | 23.50 ± 11.61b,c |
GT | 491 ± 329 | 498 ± 349 | 489 ± 339 | 2.66 ± 1.82b | 2.44 ± 1.65c | 3.29 ± 2.33b,c |
Pooled | 1,452 ± 1,515 | 1,430 ± 1,457 | 1,419 ± 1,466 | 8.25 ± 8.91b | 8.16 ± 8.92c | 10.08 ± 11.14b,c |
PR model predictions different from experimental measurements;
PR model predictions different from voxel model predictions;
voxel model predictions different from experimental measurements, p<0.05.