Figure 4.

Figure 4

Photographs of the transparent-opaque transition of the PNIPAm/GO hydrogel window (left) and the PNIPAm hydrogel window (right): (a) initial state, and (b) after sunlight irradiation. (c) Thermal photographs for fabricated windows taken during outdoor switching test. (Image courtesy of Dowan Kim).