Skip to main content
. 2015 Jan 8;5:7686. doi: 10.1038/srep07686

Figure 5. SEM and TEM images of Au NPs obtained by laser irradiation (λ = 532 nm, 20 Hz) at various laser fluences for 240 s.

Figure 5