Skip to main content
. 2015 Jan 9;1376:74–83. doi: 10.1016/j.chroma.2014.12.010

Table 1.

Equilibrium binding study of the varying chemical modifications used to fabricate diethylaminoethyl (DEAE) and carboxylate (COO) cellulose nanofibre adsorbents, detailing the maximum capacity of protein bound, Qmax, and dissociation constant, Kd, estimated using a Langmuir linear regression fit.

Sample DEAE cellulose
COO cellulose
Reactant conc. 50 mmol 200 mmol 2× 200 mmol 5 mmol 10 mmol 20 mmol
Qmax (mg/mL) 7.5 13.0 27.4 11.8 18.9 47.5
Kd (mg/mL) 0.077 0.044 0.11 0.065 0.034 0.049