Skip to main content
. 2014 Oct 1;21(1-2):382–389. doi: 10.1089/ten.tea.2014.0083

Table 1.

Composition of the Bioactive Glass Used in This Study

BGs SiO2 (mol%) P2O5 (mol%) CaO (mol%) Na2O (mol%) CoO (mol%)
BG0Co 49.46 1.07 23.08 26.38  
BG0.5Co 49.46 1.07 22.58 26.38 0.50
BG1Co 49.46 1.07 22.08 26.38 1.00
BG2Co 49.46 1.07 21.08 26.38 2.00
BG4Co 49.46 1.07 19.08 26.38 4.00

BG, bioactive glass.