. 2015 Jan 19;10:765–774. doi: 10.2147/IJN.S66058

Figure 4.

Figure 4

X-ray diffraction patterns of sulphated zirconia calcined at 600°C for 3 hours.

Notes: ○, monoclinic phase; ♦, tetragonal phase of zirconia.