Figure 4.

Figure 4

Images of specimens after lap shear testing. While the blends with lower T1107 ACR/NHS content (100:0 and 75:25) mainly failed due to detachment of the adhesive from the tissue (adhesive failure, A), the blends with higher T1107 ACR/NHS content (50:50 and 25:75) mainly failed due to tearing of the adhesive (cohesive failure, B).