Skip to main content
. 2014 May 13;53(27):7048–7052. doi: 10.1002/anie.201400600

Table 1.

Textural properties of IWW and its post-synthesis modified forms evaluated from argon adsorption measured at −186 °C.

Si/Ge Argon adsorption
(EDX) BET [m2 g−1] Vmic[a] [cm3 g−1] Vtot[b] [cm3 g−1]
Parent IWW 3.1 416.1 0.169 0.484
Hydrolyzed (IPC-5) 45.86 123.6 0.030 0.213
Surfactant-treated (IPC-5SW calcined) 278.5 0.015 0.278
Restored IWW 73.38 509.5 0.146 0.450

[a] Micropore volume. [b] Total pore volume.