Skip to main content
. 2015 Feb 13;56(2):1070–1080. doi: 10.1167/iovs.14-15997

Figure 1.

Figure 1

(A) Scanning electron microscope images of a sample of freshly etched pSi microparticles. (B) A close-up SEM view of one of the microparticles, showing the mesoporous structure.