Skip to main content
. Author manuscript; available in PMC: 2016 Apr 1.
Published in final edited form as: J Tissue Eng Regen Med. 2012 Dec 18;9(4):368–374. doi: 10.1002/term.1678

Figure 1.

Figure 1

Immunoblot of phosphorylated ERK (P-ERK) with hydrostatic pressure (HP) treatment. Assembled from a single larger gel, equal amounts of protein were loaded per lane. Hydrostatic pressure induced ERK activation in self-assembled constructs at day 10 and weakly at day 14.