Skip to main content
. 2015 Feb 19;15(1):9. doi: 10.1186/s12896-015-0123-2

Figure 2.

Figure 2

AFM topographic images of spidroin-based biopolymer layers. Surfaces have been taken in the intermitting tapping mode using 2.5 × 2.5 μm2 scan sizes of A) 1xVSO1-100xELP, B) 2xVSO1-100xELP and C) 4xVSO1-100xELP.