Skip to main content
. 2014 Sep 26;21(3):263–273. doi: 10.1089/ten.tec.2014.0224

FIG. 1.

FIG. 1.

A schematic outlining of the three steps involved in fabricating cell-laden macroporous OPF hydrogels. The hydrogel precursor solution was first mixed with cells and dehydrated gelatin microspheres at 23°C. The mixture was then incubated at 23°C to allow for OPF gelation and the gel was finally incubated at 37°C for gelatin leaching and hydrogel swelling. OPF, oligo(poly(ethylene glycol) fumarate).