Figure 5.

SEM micrographs of samples with 20 wt% Ni loading: (a) oxide precursor for Ni on the foam surface and (b) Ni on the foam surface, obtained after reduction of oxide precursor at 633 K.

SEM micrographs of samples with 20 wt% Ni loading: (a) oxide precursor for Ni on the foam surface and (b) Ni on the foam surface, obtained after reduction of oxide precursor at 633 K.